Refine
Document Type
- Conference Proceeding (31)
- Article (13)
- Other Publications (7)
- Book (2)
- Part of a Book (1)
Language
- English (29)
- German (24)
- Multiple languages (1)
Has Fulltext
- no (54) (remove)
Keywords
- Abrasive grain material (1)
- Actuators (1)
- Aktuatorik (1)
- Anhaftung (1)
- Aquaculture (1)
- Aufsatzsammlung (1)
- Austenitic stainless steels (1)
- Behälterbau (1)
- Biokompatibilität (1)
- Chemische Beständigkeit (1)
Characterization of NiTi Shape Memory Damping Elements designed for Automotive Safety Systems
(2014)
Actuator elements made of NiTi shape memory material are more and more known in industry because of their unique properties. Due to the martensitic phase change, they can revert to their original shape by heating when subjected to an appropriate treatment. This thermal shape memory effect (SME) can show a significant shape change combined with a considerable force. Therefore such elements can be used to solve many technical tasks in the field of actuating elements and mechatronics and will play an increasing role in the next years, especially within the automotive technology, energy management, power, and mechanical engineering as well as medical technology. Beside this thermal SME, these materials also show a mechanical SME, characterized by a superelastic plateau with reversible elongations in the range of 8%. This behavior is based on the building of stress-induced martensite of loaded austenite material at constant temperature and facilitates a lot of applications especially in the medical field. Both SMEs are attended by energy dissipation during the martensitic phase change. This paper describes the first results obtained on different actuator and superelastic NiTi wires concerning their use as damping elements in automotive safety systems. In a first step, the damping behavior of small NiTi wires up to 0.5 mm diameter was examined at testing speeds varying between 0.1 and 50 mm/s upon an adapted tensile testing machine. In order to realize higher testing speeds, a drop impact testing machine was designed, which allows testing speeds up to 4000 mm/s. After introducing this new type of testing machine, the first results of vertical-shock tests of superelastic and electrically activated actuator wires are presented. The characterization of these high dynamic phase change parameters represents the basis for new applications for shape memory damping elements, especially in automotive safety systems.
This paper compares the surface morphology of differently finished austenitic stainless steel AISI 316L, also in combination with low temperature carburization. Milled and tumbled surfaces were analyzed by means of corrosion resistance and surface morphology. The results of potentiodynamic measurements show that professional grinding operations with SiC and Al2O3 always lead to a better corrosion resistance of low temperature carburized surfaces compared to the untreated reference in the used acidified chloride solution. Big influence on the corrosion resistance of vibratory ground or tumbled surfaces has the amount of plastic deformation while machining, that has to be kept low for austenitic stainless steels. Due to the high ductility, plastic deformation can lead to the formation of meta stable pits that can be initiation points of corrosion. The formation of meta stable pits can be aggravated by low temperature diffusion processes.
Differences in the pitting resistance between cold worked CrNi and CrNiMnN metastable austenites
(2015)
Fachvortrag auf dem Kongress CORROSION 2015, 15-19 March, Dallas, Texas, USA. NACE International
Hot isostatic pressing (HIP) allows the production of complex components geometry. Generally, a high quality of the components is achieved due to the well managed composition of the metal powder and the non-isotropic properties. If a duplex stainless steel is produced, a heat treatment after the HIP-process is necessary to remove precipitations like carbides, nitrides and intermetallic phases. In a new process, the sintering step should be combined with the heat treatment. In this case a high cooling rate is necessary to avoid precipitations in duplex stainless steels. In this work, the influence of the HIP-temperature and the wall thickness on corrosion resistance, microstructure and impact strength were investigated. The results should help to optimize the process parameters like temperature and cooling rate. For the investigation, two HIP-temperatures were tested in a classical HIP-process step with a defined cooling rate. An additional heat treatment was not conducted. The specimens were cut from different sectors of the HIP-block. For investigation of the corrosion resistance, the critical pitting temperature was determined with electrochemical method according to EN ISO 17864. An impact test was used to determine the impact transition temperature. Metallographic investigations show the microstructure in the different sectors of the HIP-block.
The corrosion resistance of stainless steels is massively influenced by the condition of their surface. The surface quality includes the topography of the surface, the structure and composition of the passive layer, and the surface near structure of the base material. These factors are influenced by final physical/chemical surface treatments. The presented work shows significantly lower corrosion resistance for mechanical machined specimens than for etched specimens. It also turns out that the rougher the surface, the lower the corrosion resistance gets. However, there is no general finding which shows if blasted or grinded surfaces are more appropriate, but a dependency on process parameters and the characteristics on corrosive exposure in terms of corrosion behavior. The results show that not only the surface roughness Ra has an influence on corrosion behavior but also the shape of peaks and valleys which are evolved by surface treatments. Imperfections in the base material, like sulfidic inclusions lead to a weaker passive layer, respectively, to a decrease of the corrosion resistance. By using special passivating techniques the corrosion resistance of stainless steels can be increased to a higher level in comparison to common passivation.
Corrosion
(2016)
Rostfreie Stähle
(2016)
Das Buch gibt einen Überblick über die metallkundlichen Grundlagen auf dem Gebiet der nichtrostenden Stähle und über das Einsatzverhalten dieser Werkstoffe. Es werden die notwendigen Hinweise für den Konstrukteur und den Verarbeiter von nichtrostenden Stählen gegeben. Einen Schwerpunkt stellt hierbei das Korrosionsverhalten dieser Werkstoffe dar.
The electrochemical behavior for different surface conditions and different degrees of deformation of metastable austenitic stainless steel AISI 304 UNS S30400 were studied using critical pitting potential and electrochemical noise measurements. The influence on corrosion resistance by using different abrasives (silicon carbide and corundum) for surface finish by grinding is illustrated. For the characterization of local defects and surface topography, scanning electron microscopy (SEM) and tactile measurements were used. An inverse correlation between occurrence of local defects on the surface and critical pitting potential was found by using image processing. Therefore, gray scale values of different surfaces were compared. The influence of mass content of α'-martensite on the corrosion resistance is shown by comparing different qualities of surface finish. For smooth machined surfaces it can be shown that an increasing numbers of strain induced martensite is decreasing the corrosion resistance lightly. For low abrasive machining an inverse correlation between the critical pitting potential and surface roughness is given. However, for higher abrasive machining parameters, this correlation could not be found.